1.7765 Tool Die Steels

1.7765 - Specification & Application

Chemical composition(wt.%) of 1.7765 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C(CarBon) - 0.35
Cr - 3.0
Mo - 1.0
V - 0.25

1.7765 - Detail

32CrMoV12-10

Mechanical properties of grade 1.7765

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
635 (≥) 637 (≥) 32 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade 1.7765

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
115 (≥) 929 (≥) 41 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
312 683 843

Equivalent Products

We can customize the production of 1.7765 grade, contact us for the best solution.