10X13M Stainless Steels

10X13M - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 10X13M grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.15
Si - 0.60
Mn - 0.60
P - 0.030
S - 0.025
Cr 12.00 14.00
Ni - 0.60
Mo 1.00 1.60
Ti 2.60 3.20
Al - 0.12
B - 0.010

10X13M - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 10X13M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
846 (≥) 271 (≥) 42 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade 10X13M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
655 (≥) 467 (≥) 43 33 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
471 195 754

Equivalent Grade

Equivalent Products

We can customize the production of 10X13M grade, contact us for the best solution.
sales@specificsteel.com