11X17H Stainless Steels

11X17H - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 11X17H grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.13
Si 0.40 0.80
Mn - 0.60
P - 0.035
S - 0.020
Cr 15.60 17.60
Ni 0.90 1.40
Mo - -

11X17H - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 11X17H

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
574 (≥) 641 (≥) 44 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade 11X17H

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
289 (≥) 282 (≥) 24 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
684 741 236