Chemical composition(wt.%) of 12Cr12Mo / 1Cr12Mo grade: to GB/T 8732-2014

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.15
Si - 0.50
Mn 0.30 0.60
P - 0.030
S - 0.020
Ni 0.30 0.60
Cr 11.50 13.00
Mo 0.30 0.60
Cu - 0.30

12Cr12Mo / 1Cr12Mo - Detail

12Cr12Mo 1Cr12Mo

Mechanical properties of grade 12Cr12Mo / 1Cr12Mo GB/T 8732-2014

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
749 (≥) 644 (≥) 14 42 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade 12Cr12Mo / 1Cr12Mo GB/T 8732-2014

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
264 (≥) 989 (≥) 13 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
839 872 323