12X18H12T Stainless Steels

12X18H12T - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 12X18H12T grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.80
Mn - 2.00
P - 0.035
S - 0.020
Cr 17.00 19.00
Ni 11.00 13.00
Mo - 0.30
W - 0.20
Ti 5×C 0.70

12X18H12T - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 12X18H12T

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
779 (≥) 735 (≥) 23 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade 12X18H12T

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
613 (≥) 214 (≥) 41 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
699 414 818

Equivalent Grade

Equivalent Products

We can customize the production of 12X18H12T grade, contact us for the best solution.
sales@specificsteel.com