13X14H382ΦP Stainless Steels

13X14H382ΦP - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 13X14H382ΦP grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.16
Si - 0.60
Mn - 0.60
P - 0.030
S - 0.025
Cr 13.00 15.00
Ni 2.80 3.40
Mo - 0.30
W - 0.20
Ti - 0.05
V 0.18 0.28
B - 0.0040

13X14H382ΦP - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 13X14H382ΦP

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
552 (≥) 981 (≥) 13 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade 13X14H382ΦP

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
443 (≥) 558 (≥) 41 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
684 258 135

Equivalent Grade

Equivalent Products

We can customize the production of 13X14H382ΦP grade, contact us for the best solution.