15X12BHMΦ Special Alloy

Chemical composition%of the ladle analysis of grade15X12BHMΦ

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Mo(%)V(%)W(%)Ti(%)
0.12-0.18Max 0.400.50-0.90Max 0.03Max 0.02511.0-13.00.40-0.800.50-0.700.15-0.300.70-1.10Max 0.20
15X12BHMΦ

Mechanical properties of grade15X12BHMΦ

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
356(≥) 454(≥) 12 12 12 Solution and Aging,Annealing,Ausaging,Q+T,etc 443

Physical properties of grade 15X12BHMΦ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
847(≥) 521(≥) 23 41 21 Solution and Aging,Annealing,Ausaging,Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
413 128 627

15X12BHMΦ Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting