1Cr13Mn9Ni4 Stainless Steels

1Cr13Mn9Ni4 - Specification & Application

1Cr13Mn9Ni4

Chemical composition(wt.%) of 1Cr13Mn9Ni4 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.25
Si - 1.00
Mn 8.00 10.00
P - 0.035
S - 0.030
Ni 3.75 5.00
Cr 12.00 14.00

1Cr13Mn9Ni4 - Detail

1Cr13Mn9Ni4

Mechanical properties of grade 1Cr13Mn9Ni4

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
633 (≥) 551 (≥) 34 41 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade 1Cr13Mn9Ni4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
748 (≥) 854 (≥) 41 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
625 159 132