Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.17 | 0.23 | ||
Si | - | 0.60 | ||
Mn | 0.50 | 0.90 | ||
P | - | 0.030 | ||
S | - | 0.025 | ||
Cr | 10.50 | 12.50 | ||
Ni | 0.50 | 0.90 | ||
Mo | 0.50 | 0.70 | ||
W | - | 0.20 | ||
Ti | - | - | ||
V | 0.15 | 0.30 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
793 (≥) | 387 (≥) | 42 | 23 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 112 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
992 (≥) | 142 (≥) | 41 | 24 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
124 | 768 | 218 |
We can customize the production of 20X12BHMΦ grade, contact us for the best solution.