2HR501 Stainless Steels to BS 2HR 501 (1973)

2HR501 - Specification & Application

  • BS 2HR 501 (1973) - Specification for nickel-chromium-cobalt-titanium-aluminium heat-resisting alloy cold drawn wire for springs (nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)
  • BS 3HR 501 (2011) - Specification for nickel-chromium-cobalt-titanium- aluminium heat-resisting alloy cold drawn wire for springs and springs (Nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)

Specification for nickel-chromium-cobalt-titanium- aluminium heat-resisting alloy cold drawn wire for springs and springs (Nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)

Chemical composition(wt.%) of 2HR501 grade: to BS 2HR 501 (1973)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.13
Si - 1.00
Mn - 1.00
P - -
S - 0.015
Cr 18.00 21.00
Ni - remaining
Mo - -
Co 15.00 21.00
Ti 2.00 3.00
Fe - 1.50
Al 1.00 2.00
Cu - 0.20
Zr - 0.15
B - 0.020
Bi - 0.0001
Pb - 0.002
Ag - 0.0005

2HR501 - Detail

Specification for nickel-chromium-cobalt-titanium- aluminium heat-resisting alloy cold drawn wire for springs and springs (Nickel base, Cr 19.5, Co 18.0, Ti 2.5, Al 1.5)

Mechanical properties of grade 2HR501 BS 2HR 501 (1973)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
824 (≥) 263 (≥) 13 41 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade 2HR501 BS 2HR 501 (1973)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
394 (≥) 514 (≥) 43 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 423
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
132 849 912

Equivalent Grade

Equivalent Products

We can customize the production of 2HR501 grade, contact us for the best solution.
sales@specificsteel.com