303 Cu Stainless Steels to SAE J 405 (1998)

303 Cu - Specification & Application

  • SAE J 405 (1998) - Chemical compositions of SAE wrought stainless steels

Chemical compositions of SAE wrought stainless steels

Chemical composition(wt.%) of 303 Cu grade: to SAE J 405 (1998)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.15
S 0.10 -
Cr 17.0 19.0
Ni 6.00 10.0
Cu 2.50 4.00
Se 0.10 -

303 Cu - Detail

Chemical compositions of SAE wrought stainless steels

Mechanical properties of grade 303 Cu SAE J 405 (1998)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
976 (≥) 857 (≥) 22 43 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade 303 Cu SAE J 405 (1998)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
163 (≥) 289 (≥) 31 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
166 637 936