304L Stainless Steels to MIL-DTL-23196E

304L - Specification & Application

  • MIL-DTL-23196E - Steel plate, corrosion resistant, austenitic (UNS S30400, S30403, S31600, S34700, and S34800)
  • MIL-P-1144D - Pipe, corrosion-resistant, stainless steel, seamless or welded
  • MIL-S-23196 - Steel plate, corrosion resistant, austenitic (UNS S30400, S30403, S31600, S34700, and S34800)
  • MIL-S-4043B - Steel; Corrosion-resisting (extra low carbon type 304), plate, sheet, and strip
  • MIL-S-862B - Steel bar, corrosion resisting, and steel billet, corrosion resisting, reforging application
  • MIL-T-8973 - Tubing, steel, corrosion and heat resistant, for aerospace vehicle hydraulic systems assembled by brazing

Tubing, steel, corrosion and heat resistant, for aerospace vehicle hydraulic systems assembled by brazing

Chemical composition(wt.%) of 304L grade: to MIL-DTL-23196E

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.0 20.0
Ni 8.00 10.0
N - 0.10

304L - Detail

Tubing, steel, corrosion and heat resistant, for aerospace vehicle hydraulic systems assembled by brazing

Mechanical properties of grade 304L MIL-DTL-23196E

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
431 (≥) 182 (≥) 32 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade 304L MIL-DTL-23196E

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
276 (≥) 762 (≥) 34 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
644 323 298
We can customize the production of 304L grade, contact us for the best solution.