34CrNiMo6 Stainless Steels to NF EN 10083-1

34CrNiMo6 - Specification & Application

  • NF EN 10083-1 - Steels for quenching and tempering - Part 1: General technical delivery conditions
  • NF EN 10083-3 - Steels for quenching and tempering - Part 3: Technical delivery conditions for alloy steels
  • NF EN 10250-3 - Open die steel forgings for general engineering purposes - Part 3: Alloy special steels
  • NF EN 10263-4 - Steel rod, bars and wire for cold heading and cold extrusion - Part 4: Technical delivery conditions for steels for quenching and tempering
  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties
  • NF EN 10277-5 - Bright steel products - Technical delivery conditions - Part 5: Steels for quenching and tempering
  • NF EN 10343 - Steels for quenching and tempering for construction purposes - Technical delivery conditions

Steels for quenching and tempering for construction purposes - Technical delivery conditions

Chemical composition(wt.%) of 34CrNiMo6 grade: to NF EN 10083-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.30 0.38
Si - 0.40
Mn 0.50 0.80
P - 0.035
S - 0.035
Cr 1.30 1.70
Ni 1.30 1.70
Mo 0.15 0.30

34CrNiMo6 - Detail

Steels for quenching and tempering for construction purposes - Technical delivery conditions

Mechanical properties of grade 34CrNiMo6 NF EN 10083-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
992 (≥) 764 (≥) 21 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade 34CrNiMo6 NF EN 10083-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
676 (≥) 199 (≥) 13 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
327 324 424

Equivalent Products

We can customize the production of 34CrNiMo6 grade, contact us for the best solution.
sales@specificsteel.com