38Х2Н2МА Stainless Steels to GOST 4543

38Х2Н2МА - Specification & Application

  • GOST 4543 - Structural alloy steel bars. Specifications
  • GOST 8479 - Structural carbon and alloyed steel forgings. General specification

Structural alloy steel bars. Specifications

Chemical composition(wt.%) of 38Х2Н2МА grade: to GOST 4543

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.33 0.40
Si 0.17 0.37
Mn 0.25 0.50
Ni 1.30 1.70
S - 0.025
P - 0.025
Cr 1.3 1.7
Mo 0.20 0.30
Cu - 0.30

38Х2Н2МА - Detail

Mechanical properties of grade 38Х2Н2МА GOST 4543

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
795 (≥) 593 (≥) 33 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade 38Х2Н2МА GOST 4543

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
657 (≥) 411 (≥) 24 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 242
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
531 953 878

Equivalent Grade

Equivalent Products

We can customize the production of 38Х2Н2МА grade, contact us for the best solution.