416S37 Stainless Steels to BS 970-1

416S37 - Specification & Application

  • BS 970-1 - Specification for wrought steels for mechanical and allied engineering purposes. General inspection and testing procedures and specific requirements for carbon, carbon manganese, alloy and stainless steels
  • BS 970-3 - Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Chemical composition(wt.%) of 416S37 grade: to BS 970-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 0.28
Si - 1.00
Mn - 1.50
P - 0.06
S 0.15 0.35
Cr 12.00 14.00
Mo - 0.60
Ni - 1.00

416S37 - Detail

Specification for wrought steels for mechanical and allied engineering purposes. Bright bars for general engineering purposes

Mechanical properties of grade 416S37 BS 970-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
762 (≥) 919 (≥) 34 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade 416S37 BS 970-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
539 (≥) 426 (≥) 33 13 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
699 227 798

Equivalent Grade

Equivalent Products