42CrMo5-6 Stainless Steels to NF EN 10269

42CrMo5-6 - Specification & Application

  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Chemical composition(wt.%) of 42CrMo5-6 grade: to NF EN 10269

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.39 0.45
Si - 0.40
Mn 0.40 0.70
P - 0.035
S - 0.035
Cr 1.20 1.50
Ni - -
Mo 0.50 0.70

42CrMo5-6 - Detail

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Mechanical properties of grade 42CrMo5-6 NF EN 10269

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
155 (≥) 868 (≥) 14 21 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade 42CrMo5-6 NF EN 10269

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
641 (≥) 824 (≥) 32 42 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
646 951 117

Equivalent Products

We can customize the production of 42CrMo5-6 grade, contact us for the best solution.
sales@specificsteel.com