4Cr9Si2 Stainless Steels to GB/T 1221 (1992)

4Cr9Si2 - Specification & Application

  • GB/T 1221 (1992) - Heat-resisting steel bars
  • GB/T 12773 (1991) - Valve steel bars for internal combustion engines - Technical requirements
  • JB/T 6398 (2006) - Heavy stainless acid resistant and heat resistant steel forgings

Valve steel bars for internal combustion engines - Technical requirements

Chemical composition(wt.%) of 4Cr9Si2 grade: to GB/T 1221 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.50
Si 2.00 3.00
Mn - 0.70
P - 0.035
S - 0.030
Ni - 0.60
Cr 8.00 10.00

4Cr9Si2 - Detail

4Cr9Si2

Mechanical properties of grade 4Cr9Si2 GB/T 1221 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
654 (≥) 914 (≥) 22 44 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade 4Cr9Si2 GB/T 1221 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
164 (≥) 741 (≥) 34 14 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
994 971 895

Equivalent Grade

Equivalent Products