59CrV4 Tool Die Steels

59CrV4 - Specification & Application

Alloyed CrV steel

Chemical composition(wt.%) of 59CrV4 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.55 0.62
Si 0.15 0.35
Mn 0.80 1.10
P - 0.035
S - 0.035
Cr 0.90 1.20
Mo - -
V 0.07 0.12

59CrV4 - Detail

Alloyed CrV steel

Mechanical properties of grade 59CrV4

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
833 (≥) 813 (≥) 11 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade 59CrV4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
744 (≥) 283 (≥) 32 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
645 331 468

Equivalent Grade

Equivalent Products

We can customize the production of 59CrV4 grade, contact us for the best solution.