6Cr4W3Mo2VNb Special Alloy

Chemical composition%of the ladle analysis of grade6Cr4W3Mo2VNb

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Mo(%)V(%)W(%)Nb(%)
0.60~0.70≤0.40≤0.40≤0.030≤0.0303.80~4.401.80~2.500.80~1.202.50~3.500.20~0.35
  • » Alloy steel the performance characteristic and the USES(4)
  • » Alloy steel the performance characteristic and the USES(3)
  • » Alloy steel the performance characteristic and the USES(2)
  • » Alloy steel the performance characteristic and the USES(1)
  • Mechanical properties of grade6Cr4W3Mo2VNb

    Proof strength
    Rp0.2(MPa)
    Tensile strength
    Rm(MPa)
    Impact energy
    KV(J)
    Elongation at fracture
    A(%)
    Reduction in cross section on fracture
    Z(%)
    As-Heat-Treated Condition Brinell hardness(HBW)
    526(≥) 357(≥) 33 34 33 Solution and Aging,Annealing,Ausaging,Q+T,etc 241

    Physical properties of grade 6Cr4W3Mo2VNb

    Property Density
    kg/dm3
    Temperature T
    °C/F
    Specific heat
    J/kgK
    Thermal conductivity
    W/mK
    Electric resistance
    µΩ·cm
    Modulus of elasticity
    kN/mm2
    Expansion rate
    911(≥) 915(≥) 22 14 14 Solution and Aging,Annealing,Ausaging,Q+T,etc 114
    Temp.
    °C/°F
    Creep strain limit
    (10000h)
    (Rp1,0)N/mm2
    Creep rupture strength
    (10000h)
    (Rp1,0)N/mm2
    642 464 972

    6Cr4W3Mo2VNb Range of products

    Product type Products Dimension Processes Deliver Status
    Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
    Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
    Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
    Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

    Equivalent Grade