Ball and Roller Bearing Steels; Technical Conditions of Delivery
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.77 | 1.85 | ||
Si | - | 0.25 | ||
Mn | - | 0.35 | ||
P | - | - | ||
S | - | - | ||
Cr | 3.75 | 4.25 | ||
Mo | 4.00 | 4.50 | ||
V | 0.90 | 1.10 |
Ball and Roller Bearing Steels; Technical Conditions of Delivery
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
594 (≥) | 448 (≥) | 13 | 23 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
515 (≥) | 391 (≥) | 32 | 44 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 213 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
588 | 937 | 651 |
We can customize the production of 81MoCrV42-16 grade, contact us for the best solution.