A 1049 S32205 Stainless Steels to A 1049/A 1049M (2010)

A 1049 S32205 - Specification & Application

  • A 1049/A 1049M (2010) - Stainless Steel Forgings, Ferritic/Austenitic (Duplex), for Pressure Vessels and Related Components

Stainless Steel Forgings, Ferritic/Austenitic (Duplex), for Pressure Vessels and Related Components

Chemical composition(wt.%) of A 1049 S32205 grade: to A 1049/A 1049M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.03
S - 0.02
Cr 22.00 23.00
Ni 4.50 6.50
Mo 3.00 3.50
N 0.14 0.20

A 1049 S32205 - Detail

Stainless Steel Forgings, Ferritic/Austenitic (Duplex), for Pressure Vessels and Related Components

Mechanical properties of grade A 1049 S32205 A 1049/A 1049M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
222 (≥) 526 (≥) 11 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade A 1049 S32205 A 1049/A 1049M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
336 (≥) 642 (≥) 22 32 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
713 891 742

Equivalent Products

We can customize the production of A 1049 S32205 grade, contact us for the best solution.