A 182 F 310MoLN Stainless Steels to A 182/A 182M (2012)

A 182 F 310MoLN - Specification & Application

  • A 182/A 182M (2012) - Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Chemical composition(wt.%) of A 182 F 310MoLN grade: to A 182/A 182M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.50
Mn - 2.00
P - 0.03
S - 0.01
Cr 24.00 26.00
Ni 21.0 23.0
N 0.10 0.16

A 182 F 310MoLN - Detail

Standard Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Mechanical properties of grade A 182 F 310MoLN A 182/A 182M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
171 (≥) 357 (≥) 21 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade A 182 F 310MoLN A 182/A 182M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
311 (≥) 824 (≥) 41 11 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
266 374 964

Equivalent Products