A 182 F 316 Stainless Steels to ASTM A 182 / A 182M

A 182 F 316 - Specification & Application

  • ASTM A 182 / A 182M - Forged low alloy and stainless steel piping components for use in pressure

Forged low alloy and stainless steel piping components for use in pressure

Chemical composition(wt.%) of A 182 F 316 grade: to ASTM A 182 / A 182M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00

A 182 F 316 - Detail

Stainless and heat resisting steels

Forged low alloy and stainless steel piping components for use in pressure

A 182 F 316

Mechanical properties of grade A 182 F 316 ASTM A 182 / A 182M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
685 (≥) 833 (≥) 12 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade A 182 F 316 ASTM A 182 / A 182M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
158 (≥) 428 (≥) 14 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
417 622 392
We can customize the production of A 182 F 316 grade, contact us for the best solution.