A 213 TP304H Stainless Steels to A 213/A 213M (2011)

A 213 TP304H - Specification & Application

  • A 213/A 213M (2011) - Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of A 213 TP304H grade: to A 213/A 213M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 2.00
P - 0.04
S - 0.03
Cr 18.0 20.0
Ni 8.00 11.0

A 213 TP304H - Detail

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Mechanical properties of grade A 213 TP304H A 213/A 213M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
443 (≥) 462 (≥) 23 24 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade A 213 TP304H A 213/A 213M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
692 (≥) 144 (≥) 43 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 222
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
966 324 242

Equivalent Products

We can customize the production of A 213 TP304H grade, contact us for the best solution.
sales@specificsteel.com