A 240 S30600 Stainless Steels to A 240/A 240M (2012)

A 240 S30600 - Specification & Application

  • A 240/A 240M (2012) - Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of A 240 S30600 grade: to A 240/A 240M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.018
Si 3.70 4.30
Mn - 2.00
P - 0.02
S - 0.02
Cr 17.0 18.5
Ni 14.0 15.5
Mo - 0.20
Cu - 0.50

A 240 S30600 - Detail

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade A 240 S30600 A 240/A 240M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
678 (≥) 919 (≥) 31 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade A 240 S30600 A 240/A 240M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
597 (≥) 192 (≥) 21 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 134
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
549 687 193

Equivalent Products

We can customize the production of A 240 S30600 grade, contact us for the best solution.