A 240 S44500 Stainless Steels to A 240/A 240M (2012)

A 240 S44500 - Specification & Application

  • A 240/A 240M (2012) - Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of A 240 S44500 grade: to A 240/A 240M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.012
Cr 19.00 21.00
Ni - 0.60
Mo - -
N - 0.03
Cu 0.30 0.60

A 240 S44500 - Detail

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade A 240 S44500 A 240/A 240M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
595 (≥) 155 (≥) 12 21 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade A 240 S44500 A 240/A 240M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
338 (≥) 879 (≥) 33 34 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
821 465 461

Equivalent Products

We can customize the production of A 240 S44500 grade, contact us for the best solution.