A 249 S32100 Stainless Steels to A 240/A 240M (2012)

A 249 S32100 - Specification & Application

  • A 240/A 240M (2012) - Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Chemical composition(wt.%) of A 249 S32100 grade: to A 240/A 240M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.03
Cr 17.00 19.00
Ni 9.00 12.00
N - 0.10

A 249 S32100 - Detail

Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Mechanical properties of grade A 249 S32100 A 240/A 240M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
789 (≥) 311 (≥) 31 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade A 249 S32100 A 240/A 240M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
411 (≥) 731 (≥) 23 43 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
423 288 419
We can customize the production of A 249 S32100 grade, contact us for the best solution.