A 312 TP316N Stainless Steels to A 312/A 312M (2012)

A 312 TP316N - Specification & Application

  • A 312/A 312M (2012) - Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Chemical composition(wt.%) of A 312 TP316N grade: to A 312/A 312M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N 0.10 0.16

A 312 TP316N - Detail

Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Mechanical properties of grade A 312 TP316N A 312/A 312M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
751 (≥) 465 (≥) 41 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade A 312 TP316N A 312/A 312M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
392 (≥) 546 (≥) 11 32 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
126 157 775

Equivalent Products

We can customize the production of A 312 TP316N grade, contact us for the best solution.
sales@specificsteel.com