A 358 S30600 Stainless Steels to A 358/A 358M (2008)

A 358 S30600 - Specification & Application

  • A 358/A 358M (2008) - Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Chemical composition(wt.%) of A 358 S30600 grade: to A 358/A 358M (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.018
Si 3.70 4.30
Mn - 2.00
P - 0.02
S - 0.02
Cr 17.0 18.5
Ni 14.0 15.5
Mo - 0.20
Cu - 0.50

A 358 S30600 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Mechanical properties of grade A 358 S30600 A 358/A 358M (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
476 (≥) 435 (≥) 34 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade A 358 S30600 A 358/A 358M (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
972 (≥) 643 (≥) 14 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
528 821 555

Equivalent Products

We can customize the production of A 358 S30600 grade, contact us for the best solution.