A 554 MT 301 Stainless Steels to A 554 (2011)

A 554 MT 301 - Specification & Application

  • A 554 (2011) - Welded Stainless Steel Mechanical Tubing

Welded Stainless Steel Mechanical Tubing

Chemical composition(wt.%) of A 554 MT 301 grade: to A 554 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.0 18.0
Ni 6.00 8.00

A 554 MT 301 - Detail

Austenitic steel; As-welded or cold-reduced mechanical tubing in sizes to 406.4 mm outside dimension, and in wall thicknesses 0.51 mm and over.
Intended for use in ornamental, structural, exhaust, and other applications where appearance, mechanical properties, or corrosion resistance is needed.

Mechanical properties of grade A 554 MT 301 A 554 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
684 (≥) 953 (≥) 42 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade A 554 MT 301 A 554 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
629 (≥) 755 (≥) 21 34 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
272 683 143