A 564 S45503 Stainless Steels to A 564/A 564M (2010)

A 564 S45503 - Specification & Application

  • A 564/A 564M (2010) - Hot-Rolled and Cold-Finished Age-Hardening Stainless Steel Bars and Shapes

Hot-Rolled and Cold-Finished Age-Hardening Stainless Steel Bars and Shapes

Chemical composition(wt.%) of A 564 S45503 grade: to A 564/A 564M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 0.50
Si - 0.20
P - 0.01
S - 0.01
Cr 11.00 12.50
Ni 7.50 9.50
Mo - 0.50

A 564 S45503 - Detail

Hot-Rolled and Cold-Finished Age-Hardening Stainless Steel Bars and Shapes

Mechanical properties of grade A 564 S45503 A 564/A 564M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
355 (≥) 585 (≥) 23 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade A 564 S45503 A 564/A 564M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
756 (≥) 374 (≥) 44 23 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
693 222 175

Equivalent Products

We can customize the production of A 564 S45503 grade, contact us for the best solution.
sales@specificsteel.com