A 582 S42023 Stainless Steels to A 582/A 582M (2012)

A 582 S42023 - Specification & Application

  • A 582/A 582M (2012) - Standard Specification for Free-Machining Stainless Steel Bars

Standard Specification for Free-Machining Stainless Steel Bars

Chemical composition(wt.%) of A 582 S42023 grade: to A 582/A 582M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.30 0.40
Mn - 1.25
Si - 1.00
P - 0.06
S - 0.06
Cr 12.00 14.00
Ni - -
Mo - -
Cu - 0.60
Zr - 0.60
Se 0.15 -

A 582 S42023 - Detail

Standard Specification for Free-Machining Stainless Steel Bars

Mechanical properties of grade A 582 S42023 A 582/A 582M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
672 (≥) 173 (≥) 12 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade A 582 S42023 A 582/A 582M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
393 (≥) 546 (≥) 24 43 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
429 324 269

Equivalent Products

We can customize the production of A 582 S42023 grade, contact us for the best solution.