A 815 CRS32950 Stainless Steels to A 815/A 815M (2010)

A 815 CRS32950 - Specification & Application

  • A 815/A 815M (2010) - Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings

Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings

Chemical composition(wt.%) of A 815 CRS32950 grade: to A 815/A 815M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 0.60
P - 0.035
S - 0.01
Cr 26.00 29.00
Ni 3.50 5.20
Mo 1.00 2.50
N 0.15 0.35

A 815 CRS32950 - Detail

Wrought Ferritic, Ferritic/Austenitic, and Martensitic Stainless Steel Piping Fittings

Mechanical properties of grade A 815 CRS32950 A 815/A 815M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
719 (≥) 887 (≥) 32 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade A 815 CRS32950 A 815/A 815M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
594 (≥) 578 (≥) 41 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
661 734 218

Equivalent Products

We can customize the production of A 815 CRS32950 grade, contact us for the best solution.