Chemical composition(wt.%) of A 831 S38660 grade: to A 831/A 831M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.03
Cr 11.50 13.50
Ni 14.00 16.00

A 831 S38660 - Detail

Austenitic and Martensitic Stainless Steel Bars, Billets, and Forgings for Liquid Metal Cooled Reactor Core Components

                                                              Standard Withdrawn

Mechanical properties of grade A 831 S38660 A 831/A 831M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
374 (≥) 335 (≥) 42 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade A 831 S38660 A 831/A 831M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
523 (≥) 978 (≥) 34 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
194 862 588