A 959 S41500 Stainless Steels to A 959 (2011)

A 959 S41500 - Specification & Application

  • A 959 (2011) - Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Chemical composition(wt.%) of A 959 S41500 grade: to A 959 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Mn 0.50 1.00
Si - 0.60
P - 0.03
S - 0.03
Cr 11.50 14.00
Ni 3.50 5.50
Mo 0.50 1.00

A 959 S41500 - Detail

Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Mechanical properties of grade A 959 S41500 A 959 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
672 (≥) 981 (≥) 43 44 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade A 959 S41500 A 959 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
481 (≥) 578 (≥) 24 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
959 441 979