A5 Tool Die Steels to ASTM A681-1999

A5 - Specification & Application

  • ASTM A681-1999 - Alloy tool steel

Alloy tool steel

Chemical composition(wt.%) of A5 grade: to ASTM A681-1999

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.05
Si 0.10 0.50
Mn 2.80 3.20
P - 0.030
S - 0.030
Cr 0.90 1.20
Mo 0.90 1.40
Ni+Cu - 0.75

A5 - Detail

A5

Mechanical properties of grade A5 ASTM A681-1999

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
894 (≥) 651 (≥) 34 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade A5 ASTM A681-1999

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
261 (≥) 596 (≥) 33 11 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
348 351 586

Equivalent Products

We can customize the production of A5 grade, contact us for the best solution.
sales@specificsteel.com