ASTM633 Stainless Steels

ASTM633 - Specification & Application

ASTM633

Chemical composition(wt.%) of ASTM633 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.07 0.11
Si - 0.50
Mn 0.50 1.25
P - 0.04
S - 0.03
Cr 16.0 17.0
Ni 4.00 5.00
Mo 1.25 2.5
N 0.07 0.13

ASTM633 - Detail

ASTM633

Mechanical properties of grade ASTM633

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
398 (≥) 587 (≥) 31 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade ASTM633

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
458 (≥) 617 (≥) 11 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
286 339 214

Equivalent Products

We can customize the production of ASTM633 grade, contact us for the best solution.