ASTMXM-12 Stainless Steels

ASTMXM-12 - Specification & Application

ASTMXM-12

Chemical composition(wt.%) of ASTMXM-12 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
c - 0.07
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 14.0 15.5
Ni 3.50 5.50
Cu 2.50 4.50
Nb 0.15 0.45

ASTMXM-12 - Detail

ASTMXM-12

Mechanical properties of grade ASTMXM-12

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
584 (≥) 451 (≥) 32 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade ASTMXM-12

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
252 (≥) 636 (≥) 24 44 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
281 934 943

Equivalent Products

We can customize the production of ASTMXM-12 grade, contact us for the best solution.
sales@specificsteel.com