Aluchrom 4 18 YHf
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
Ni | - | 0.5000 | ||
Cr | 17.0000 | 19.0000 | ||
C | - | 0.0800 | ||
S | - | 0.0300 | ||
Mn | - | 0.5000 | ||
Si | - | 0.6000 | ||
Al | 3.5000 | 5.0000 | ||
Y | - | 0.1500 | ||
Zr | - | 0.1500 | ||
Hf | - | 0.1500 | ||
P | - | 0.0400 | ||
Cu | - | 0.5000 |
Aluchrom 4 18 YHf
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
633 (≥) | 767 (≥) | 43 | 41 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
499 (≥) | 814 (≥) | 44 | 12 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 221 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
382 | 971 | 951 |
We can customize the production of Aluchrom 4 18 YHf grade, contact us for the best solution.
–sales@specificsteel.com