B 591 C42200 Stainless Steels to B 591 (2009)

B 591 C42200 - Specification & Application

  • B 591 (2009) - Copper-Zinc-Tin and Copper-Zinc-Tin-Iron-Nickel Alloys Plate, Sheet, Strip, and Rolled Bar

Copper-Zinc-Tin and Copper-Zinc-Tin-Iron-Nickel Alloys Plate, Sheet, Strip, and Rolled Bar

Chemical composition(wt.%) of B 591 C42200 grade: to B 591 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.22
Si - 0.40
Mn - 0.75
P - -
S - -
Ni - 0.75
Cr - 12.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - 1.00
W - 1.00
V - 0.22

B 591 C42200 - Detail

Copper-Zinc-Tin and Copper-Zinc-Tin-Iron-Nickel Alloys Plate, Sheet, Strip, and Rolled Bar

Mechanical properties of grade B 591 C42200 B 591 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
258 (≥) 989 (≥) 22 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade B 591 C42200 B 591 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
732 (≥) 248 (≥) 31 11 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
544 537 487
We can customize the production of B 591 C42200 grade, contact us for the best solution.