HNV8 Stainless Steels

HNV8 - Specification & Application

Steel for intake valves

Chemical composition(wt.%) of HNV8 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 0.25
Si - 0.50
Mn 0.50 1.00
P 0.040
S 0.025
Cr 11.0 12.5
Ni 0.50 1.00
Mo 0.90 1.25
W 0.90 1.25

HNV8 - Detail

Steel for intake valves

Mechanical properties of grade HNV8

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
943 (≥) 794 (≥) 31 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade HNV8

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
754 (≥) 396 (≥) 32 31 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
172 282 433
We can customize the production of HNV8 grade, contact us for the best solution.