C45W Tool Die Steels

C45W - Specification & Application

High carbon steel

Chemical composition(wt.%) of C45W grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.50
Si 0.15 0.40
Mn 0.60 0.80
P - 0.035
S - 0.035

C45W - Detail

High carbon steel

Mechanical properties of grade C45W

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
652 (≥) 334 (≥) 23 34 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade C45W

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
995 (≥) 396 (≥) 24 22 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
753 747 554

Equivalent Grade

Equivalent Products

We can customize the production of C45W grade, contact us for the best solution.
sales@specificsteel.com