Custom 450 Stainless Steels to SAE AMS 5763D (2010)

Custom 450 - Specification & Application

  • SAE AMS 5763D (2010) - Steel, Corrosion Resistant Bars, Forgings, Tubing, and Rings 15Cr - 6.5Ni - 0.75Mo - 0.50 (Cb + Ta) - 1.5Cu Solution Heat Treated

Steel, Corrosion Resistant Bars, Forgings, Tubing, and Rings 15Cr - 6.5Ni - 0.75Mo - 0.50 (Cb + Ta) - 1.5Cu Solution Heat Treated

Chemical composition(wt.%) of Custom 450 grade: to SAE AMS 5763D (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 1.00
Mn - 1.00
P - -
S - -
Ni 5.00 7.00
Cr 14.00 16.00
Al - -
Cu 1.25 1.75
Ti - -
Fe - -
Mo 0.50 1.00
Co - -
Nb - -

Custom 450 - Detail

Steel, Corrosion Resistant Bars, Forgings, Tubing, and Rings 15Cr - 6.5Ni - 0.75Mo - 0.50 (Cb + Ta) - 1.5Cu Solution Heat Treated

Mechanical properties of grade Custom 450 SAE AMS 5763D (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
478 (≥) 181 (≥) 14 42 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade Custom 450 SAE AMS 5763D (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
887 (≥) 712 (≥) 11 41 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
244 599 178

Equivalent Products

We can customize the production of Custom 450 grade, contact us for the best solution.