D6AC Stainless Steels to SAE AMS 6431N (2012)

D6AC - Specification & Application

  • SAE AMS 6431N (2012) - Steel, Bars, Forgings, and Tubing 1.05Cr - 0.55Ni - 1.0Mo - 0.11V (0.45 - 0.50C) Vacuum Consumable Electrode Remelted

Steel, Bars, Forgings, and Tubing 1.05Cr - 0.55Ni - 1.0Mo - 0.11V (0.45 - 0.50C) Vacuum Consumable Electrode Remelted

Chemical composition(wt.%) of D6AC grade: to SAE AMS 6431N (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.47
Si - 0.22
Mn - 0.75
P - -
S - -
Ni - 0.55
Cr - 1.05
Al - -
Cu - -
Ti - -
Fe - remaining
Mo - 1.00
Co - -
V - 0.10

D6AC - Detail

Steel, Bars, Forgings, and Tubing 1.05Cr - 0.55Ni - 1.0Mo - 0.11V (0.45 - 0.50C) Vacuum Consumable Electrode Remelted

Mechanical properties of grade D6AC SAE AMS 6431N (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
477 (≥) 122 (≥) 14 34 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade D6AC SAE AMS 6431N (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
984 (≥) 696 (≥) 21 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
423 853 741

Equivalent Products

We can customize the production of D6AC grade, contact us for the best solution.