EVl6 Stainless Steels

EVl6 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of EVl6 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.33 -
Si 0.70 -
Mn 3.00 -
P - -
S - -
Cr 23.0 -
Ni 8.00 -
N 0.38 -

EVl6 - Detail

Steel for exhaust valves

Mechanical properties of grade EVl6

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
591 (≥) 482 (≥) 43 22 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade EVl6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
417 (≥) 719 (≥) 22 22 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
646 889 632

Equivalent Grade

Equivalent Products

We can customize the production of EVl6 grade, contact us for the best solution.