GH1140 Stainless Steels to GB/T 14992 (2005)

GH1140 - Specification & Application

  • GB/T 14992 (2005) - Classification and designation for superalloys and high temperature intermetallic materials
  • GB/T 14995 (2010) - Hot-rolled superalloy sheets
  • GB/T 14996 (2010) - Cold-Rolled heat-resisting superalloy sheets
  • GB/T 14998 (1994) - Heat-resisting superalloy blanks for forged rings
  • GB/T 15062 (2008) - Superalloy tube for general application

Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(wt.%) of GH1140 grade: to GB/T 14992 (2005)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.06 0.12
Cr 20.0 23.0
Mo 2.00 2.50
Ni 35.0 40.0
W 1.40 1.80
Al 0.20 0.60
Ti 0.70 1.20
Si 0.80 0.70
P - 0.025
S - 0.015
Ce - 0.05

GH1140 - Detail

GH1140

Mechanical properties of grade GH1140 GB/T 14992 (2005)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
999 (≥) 383 (≥) 31 31 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade GH1140 GB/T 14992 (2005)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
319 (≥) 176 (≥) 13 21 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
991 936 443

Equivalent Grade

Equivalent Products

We can customize the production of GH1140 grade, contact us for the best solution.