GH4180 Superalloys

GH4180 - Specification & Application

Nickel-base superalloy

Chemical composition(wt.%) of GH4180 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Cr 18.0 21.0
Ni - Remainder
Co - 2.0
Al 1.0 1.8
Ti 1.8 2.7
B - 0.008
Fe - 1.5

GH4180 - Detail

GH4180

Mechanical properties of grade GH4180

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
516 (≥) 232 (≥) 23 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade GH4180

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
415 (≥) 828 (≥) 22 23 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
676 839 188

Equivalent Grade

Equivalent Products

We can customize the production of GH4180 grade, contact us for the best solution.
sales@specificsteel.com