HEV3 Stainless Steels

HEV3 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of HEV3 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.03 0.10
Si - 0.50
Mn - 0.50
P - 0.015
S - 0.015
Cr 14.0 17.0
Ni - remaining
Mo - 0.50

HEV3 - Detail

Steel for exhaust valves

Mechanical properties of grade HEV3

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
297 (≥) 812 (≥) 12 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade HEV3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
436 (≥) 186 (≥) 44 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
344 394 674

Equivalent Products

We can customize the production of HEV3 grade, contact us for the best solution.
sales@specificsteel.com