HEV6 Stainless Steels

HEV6 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of HEV6 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 1.50
Mn - 1.00
P - -
S - -
Cr - 20.0
Ni - remaining

HEV6 - Detail

Steel for exhaust valves

Mechanical properties of grade HEV6

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
169 (≥) 822 (≥) 34 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade HEV6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
634 (≥) 152 (≥) 34 42 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 224
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
291 646 757