HNV6 Stainless Steels

HNV6 - Specification & Application

Steel for intake valves

Chemical composition(wt.%) of HNV6 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.75 0.85
Si 1.75 2.50
Mn - 0.80
P 0.040
S 0.03
Cr 19.0 21.0
Ni 1.00 1.7
Mo 0.5 -

HNV6 - Detail

Steel for intake valves

Mechanical properties of grade HNV6

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
931 (≥) 733 (≥) 11 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade HNV6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
217 (≥) 523 (≥) 41 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
742 367 215

Equivalent Products

We can customize the production of HNV6 grade, contact us for the best solution.